Hydrogen environment embrittlement.Hydrogen embrittlement is classified into three types: internal reversible hydrogen embrittlement, hydrogen reaction embrittlement, and hydrogen environment embrittlement. Characteristics of and materials embrittled by these types of hydrogen embrittlement are discussed. Hydrogen environment embrittlement is reviewed in detail. Factors involved in standardizing test methods for detecting the occurrence of and evaluating the severity of hydrogen environment embrittlement are considered. The effects of test technique, hydrogen pressure, purity, strain rate, stress concentration factor, and test temperature are discussed.
Document ID
19720053974
Acquisition Source
Legacy CDMS
Document Type
Conference Paper
Authors
Gray, H. R.
(NASA Lewis Research Center Cleveland, Ohio, United States)
Date Acquired
August 6, 2013
Publication Date
June 1, 1972
Subject Category
Materials, Metallic
Meeting Information
Meeting: American Society for Testing and Materials, Annual Meeting
Location: Los Angeles, CA
Start Date: June 25, 1972
End Date: June 30, 1972
Sponsors: American Society for Testing and Materials
Accession Number
72A37640
Distribution Limits
Public
Copyright
Other

Available Downloads

There are no available downloads for this record.
No Preview Available