Subcritical crack growth in two titanium alloys.Measurement of subcritical crack growth during static loading of precracked titanium alloys in salt water using samples too thin for plane strain loading to predominate was examined as a method for determining the critical stress intensity for crack propagation in salt water. Significant internal crack growth followed by arrest was found at quite low stress intensities, but crack growth rates were relatively low. Assuming these techniques provided a reliable measurement of the critical stress intensity, the value for annealed Ti-4Al-1.5Mo-0.5V alloy was apparently about 35 ksi-in. to the 1/2 power, while that for annealed Ti-4Al-3Mo-1V was below 45 ksi-in. to the 1/2 power. Crack growth was also observed in tests conducted in both alloys in an air environment. At 65 ksi-in. to the 1/2 power, the extent of crack growth was greater in air than in salt water. Ti-4Al-3Mo-1V showed arrested crack growth in air at a stress intensity of 45 ksi-in. to the 1/2 power.
Document ID
19730039627
Acquisition Source
Legacy CDMS
Document Type
Reprint (Version printed in journal)
Authors
Williams, D. N.
Date Acquired
August 7, 2013
Publication Date
March 1, 1973
Publication Information
Publication: Metallurgical Transactions
Volume: 4
Subject Category
Materials, Metallic
Accession Number
73A24429
Funding Number(s)
CONTRACT_GRANT: NASW-2242
Distribution Limits
Public
Copyright
Other

Available Downloads

There are no available downloads for this record.
No Preview Available