10,000-hour cyclic oxidation behavior at 815 C /1500 F/ of 33 high-temperature alloysThirty-three commercial high-temperature Fe-, Ni-, and Co-base alloys were oxidized in air at 815 C (1500 F) for ten 1000-hour cycles. Specific weight change versus time curves were derived and the 10,000-hour surface oxides were analyzed by X-ray diffraction. The alloys were ranked by a combination of appearance and metal loss estimates derived from gravimetric data.
Document ID
19780067807
Acquisition Source
Legacy CDMS
Document Type
Conference Proceedings
Authors
Barrett, C. A. (NASA Lewis Research Center Cleveland, Ohio, United States)
Date Acquired
August 9, 2013
Publication Date
January 1, 1978
Subject Category
Metallic Materials
Meeting Information
Meeting: Conference on the Environmental degradation of engineering materials