Repeatability of mixed-mode adhesive debondingThe repeatability of debond growth rates in adhesively bonded subjected to constant-amplitude cyclic loading was studied. Debond growth rates were compared from two sets of cracked-lap-shear specimens that were fabricated by two different manufacturers and tested in different laboratories. The fabrication method and testing procedures were identical for both sets of specimens. The specimens consisted of aluminum adherends bonded with FM-73 adhesive. Critical values of strain-energy-release rate were also determined from specimens that were monotonically loaded to failure. The test results showed that the debond growth rates for the two sets of specimens were within a scatter band which is similar to that observed in fatigue crack growth in metals. Cyclic debonding occurred at strain-energy-release rates that were more than an order of magnitude less than the critical strain-energy-release rate in static tests.
Document ID
19840011497
Acquisition Source
Legacy CDMS
Document Type
Conference Paper
Authors
Everett, R. A., Jr.
(NASA Langley Research Center Hampton, VA, United States)
Johnson, W. S.
(NASA Langley Research Center Hampton, VA, United States)
Date Acquired
September 4, 2013
Publication Date
February 1, 1984
Subject Category
Nonmetallic Materials
Report/Patent Number
USAAVSCOM-TR-84-B-1
NASA-TM-85753
NAS 1.15:85753
Report Number: USAAVSCOM-TR-84-B-1
Report Number: NASA-TM-85753
Report Number: NAS 1.15:85753
Meeting Information
Meeting: ASTM Symp. on Delamination and Debonding of Mater.
Location: Pittsburgh, PA
Country: United States
Start Date: November 8, 1983
End Date: November 10, 1983
Accession Number
84N19565
Funding Number(s)
PROJECT: DA PROJ. 1L1-61102-AH-45
PROJECT: RTOP 505-33-33-05
Distribution Limits
Public
Copyright
Work of the US Gov. Public Use Permitted.
No Preview Available