NASA Logo

NTRS

NTRS - NASA Technical Reports Server

Back to Results
Surface catalytic degradation study of two linear perfluoropolyalkylethers at 345 CThin-liquid-film degradation studies of two commercially available perfluoropolyalkylether fluids (PFAE) were performed at 345 C, in nitrogen and air atmospheres, on iron and 440 C stainless steel surfaces. It was found that one fluid degraded on both iron and 440 C stainless steel surfaces in an air atmosphere, whereas the other fluid did not degrade. Chemical analysis revealed that the test fluid degraded to lower molecular weight products and that the degradation was accompanied by the formation of a brownish deposit on both the iron and 440 C stainless steel surfaces. Surface analysis of the deposit revealed a susbstantial amount of iron oxide (Fe2O3). It was hypothesized that the fluid which degraded did so because of its acetal structure. The other fluid, lacking the acetal structure, did not degrade.
Document ID
19880003161
Acquisition Source
Legacy CDMS
Document Type
Technical Publication (TP)
Authors
Morales, Wilfredo
(NASA Lewis Research Center Cleveland, OH, United States)
Date Acquired
September 5, 2013
Publication Date
November 1, 1987
Subject Category
Chemistry And Materials (General)
Report/Patent Number
NAS 1.60:2774
NASA-TP-2774
E-3395
Report Number: NAS 1.60:2774
Report Number: NASA-TP-2774
Report Number: E-3395
Accession Number
88N12543
Funding Number(s)
PROJECT: RTOP 505-63-01
Distribution Limits
Public
Copyright
Work of the US Gov. Public Use Permitted.