Elevated temperature aluminum alloysThree aluminum-lithium alloys are provided for high performance aircraft structures and engines. All three alloys contain 3 wt % copper, 2 wt % lithium, 1 wt % magnesium, and 0.2 wt % zirconium. Alloy 1 has no further alloying elements. Alloy 2 has the addition of 1 wt % iron and 1 wt % nickel. Alloy 3 has the addition of 1.6 wt % chromium to the shared alloy composition of the three alloys. The balance of the three alloys, except for incidentql impurities, is aluminum. These alloys have low densities and improved strengths at temperatures up to 260.degree. C. for long periods of time.
Document ID
20080005922
Acquisition Source
Headquarters
Document Type
Other - Patent
Authors
Meschter, Peter
Lederich, Richard J.
O'Neal, James E.
Date Acquired
August 24, 2013
Publication Date
August 29, 1989
Subject Category
Metals And Metallic Materials
Report/Patent Number
Patent Application Number: US-PATENT-APPL-SN-079316
Patent Number: US-PATENT-4,861,551
Distribution Limits
Public
Copyright
Work of the US Gov. Public Use Permitted.
Patent
US-PATENT-4,861,551