Binder for Carbon-Fiber CoatingInsoluble, even coating formed by soaking in polyacrylic acid. Carbon fiber material prepared by soaking in solution of 20 percent polyacrylic acid in water. Material blotted and dried at 120 degrees C for at least 2 hours. Dried material reacted with boiling aqueous solution of calcium acetate. Treated material removed from boiling solution, blotted, dried at 120 degrees C, washed with distilled water, and dried again.
Document ID
19830000579
Acquisition Source
Legacy CDMS
Document Type
Other - NASA Tech Brief
Authors
Dowler, W. L.
(CALTECH)
Ramohalli, K. N.
(CALTECH)
Yen, S. P. S.
(CALTECH)
Mueller, W. A.
(CALTECH)
Harper, J.
(CALTECH)
Date Acquired
August 11, 2013
Publication Date
November 1, 1984
Publication Information
Publication: NASA Tech Briefs
Volume: 8
Issue: 2
ISSN: 0145-319X
Subject Category
Materials
Report/Patent Number
NPO-14988
Accession Number
83B10579
Distribution Limits
Public
Copyright
Work of the US Gov. Public Use Permitted.

Available Downloads

There are no available downloads for this record.
No Preview Available