The response of cobalt-free Udimet 700 type alloy to modified heat treatmentsA superalloy based on Udimet 700, in which all of the cobalt was replaced by nickel, was prepared from hot isostatically pressed prealloyed powders. This material was given various heat treatments consisting of partial solutioning and aging in a sequence of four different temperatures. Comparisons were made of microstructures and mechanical properties. Best results were obtained by partially solutioning at 1145 deg C and aging through a sequence of 870, 1030, 650 and 760 deg C. This heat treatment also provided significantly improved properties for wrought material of the same composition. The results suggest that cobalt free Udimet 700 should be considered as a substitute for Udimet 700 with the standard 17 percent cobalt content.
Document ID
19860063299
Acquisition Source
Legacy CDMS
Document Type
Reprint (Version printed in journal)
External Source(s)
Authors
Harf, F. H.
(NASA Lewis Research Center Cleveland, OH, United States)
Date Acquired
August 12, 2013
Publication Date
July 1, 1986
Publication Information
Publication: Journal of Materials Science
Volume: 21
ISSN: 0022-2461
Subject Category
Metallic Materials
Accession Number
86A48037
Distribution Limits
Public
Copyright
Other

Available Downloads

There are no available downloads for this record.
No Preview Available