Polyimides containing carbonyl and ether connecting groups - IIIn a study of polyimides containing carbonyl and ether connecting groups between aromatic rings, several new polyimides were prepared and characterized. A few of these polymers were semicrystalline. Glass transition temperatures ranged from 164 to 258 C, and crystalline melt temperatures were observed between 350 and 424 C. The semicrystalline polyimide from the reaction of 3.3',4,4'-benzophenonetetracarboxylic dianhydride and 1,3-bis(4-aminophenoxy-4'-benzoyl)benzene provided transparent orange films with excellent tensile properties, exceptional resistance to solvents and strong base, and high thermooxidative stability. In addition, this polyimide provided excellent adhesive strength for joining titanium (6Al-4V) to titanium.
Document ID
19890057876
Acquisition Source
Legacy CDMS
Document Type
Reprint (Version printed in journal)
Authors
Hergenrother, P. M.
(NASA Langley Research Center Hampton, VA, United States)
Havens, S. J.
(NASA Langley Research Center Hampton, VA, United States)
Date Acquired
August 14, 2013
Publication Date
January 1, 1989
Publication Information
Publication: Journal of Polymer Science: Polymer Chemistry Edition
Volume: 27
ISSN: 0360-6376
Subject Category
Nonmetallic Materials
Accession Number
89A45247
Funding Number(s)
CONTRACT_GRANT: NAS1-18000
Distribution Limits
Public
Copyright
Other

Available Downloads

There are no available downloads for this record.
No Preview Available